Tintometer Gloss Meter TG 268 20° / 60° / 85°
Item No.
4672490
Versatile; portable gloss meter designed for fast and accurate measurement of low; medium or high gloss levels of coatings; plastics and related materials. The device is also suitable for large-scale uniformity checks in continuity mode. Basic; statistical and continuous measurement methods; Display of 5 data rows including storage capacity of more than 5000 data sets; TFT 3.5 inch; capacitive touchscreen; Intuitive; integrated software with icon guide; USB and RS 232 interfaces; Supports ASTM D523; ASTM C584; ASTM D2457; BS3900 D5; DIN 67530; DIN EN ISO 2813; EN ISO 7668 and JI Z 8741 standards; Scope of supply: Gloss meter; OnGloss software (PC); calibration plate; USB cable; external DC power supply; user manual (USB stick); carrying case; battery
Additional Details
Pack Size | ea |
Weight | 0.57 |
Weight Unit | Kg |
Additional Details
Pack Size | ea |
Weight | 0.57 |
Weight Unit | Kg |
Description
Measuring angle: 20° / 60° / 85° |
Measuring range: 20°: 0...2000 GU 60°: 0...1000 GU 85°: 0...160 GU |
Resolution: 0.1 GU | Storage: Basic Mode: 1000 | Statistical Mode: 5000 | Continuous Mode: 5000 |
Environmental conditions: 0...40 °C; 85% RH | Dimensions (W x D x H): 160 x 75 x 90 mm | Weight: 350g |
Power supply: 3200 mAh Li-ion battery |